Produced by LSR foaming, TH-series foam has a uniform microcell structure that keeps conformability and rebound force stable even in thin gauges. Five hardness grades from 30 to 45 Shore A, compression force up to 1200 kPa (25% deflection), and tensile strength to 2.0 MPa. In cell formation it balances face pressure across large areas under 1 MPa loading, with thickness loss under 10% at high temperature. UL 94 V-0 certified, 0.2–0.4 W/(m·K), rated −55°C to 200°C — ideal for dimensional-stability positioning and load-bearing pads in heavy machinery.
Properties | Test Method | Typical Value | ||||
Product | / | TH-700 | TH-800 | TH-900 | TH-1000 | TH-1000A |
Color | 目测 | 黑色 | 黑色 | 黑色 | 黑色 | 黑色 |
Density (kg/m3) | ASTM D1056 | 700~900 | 800~950 | 900~1100 | 950~1150 | 1000~1200 |
Thickness (mm) Tolerance (%) | ASTM D374/D374M / | 0.8~12.7 ±10 | 0.8~12.7 ±10 | 0.8~12.7 ±10 | 0.8~12.7 ±10 | 0.8~12.7 ±10 |
Compression Set (%) (max, 25%, 100℃, 22h) | ASTM D1056 | <5 | <5 | <5 | <5 | <5 |
Hardness (Shore A) | ASTM D2240 | 30 | 35 | 38 | 40 | 45 |
25% Compression Force Deflection (kPa) | ASTM D1056 | 500 | 900 | 950 | 1100 | 1200 |
Tensile Strength (MPa, min) | ASTM D412 | 1.3 | 1.5 | 1.7 | 2.0 | 2.0 |
Elongation at Break (%, min) | ASTM D412 | 80 | 100 | 100 | 110 | 110 |
Water Absorption (%) | ASTM D1056 | <5 | <5 | <5 | <5 | <5 |
Thermal Conductivity (W/(m·K)) | ASTM E1461 | 0.2 | 0.2 | 0.2 | 0.2 | 0.4 |
Dielectric Strength (kV/mm) | ASTM D149 | >5 | >5 | >6 | >6 | >6 |
Volume Resistivity (Ω•cm) | ASTM D257 | >1014 | >1014 | >1014 | >1014 | >1014 |
Flame Resistance | UL 94 | V-0 | V-0 | V-0 | V-0 | V-0 |
Recommended Temperature (℃ ) | SAE J-2236 | -55~200 | -55~200 | -55~200 | -55~200 | -55~200 |
Note: The above data is the average of the overall test, and we can be contacted for more product information.